Composition & manufacturing Following storage for at least 3 months, the debarked softwood logs of selected species are reduced to flakes some 10 to 30 mm in length and 0.2 to 0.3 mm in thickness using drumknife flaking machines. After passing through a hammermill, the flakes are separated into surface and core material by screening, and are then mixed with …