Grain Raising or Surface Swelling,F17 FORMPLY TECHNICAL ,formwork plywood inspection,graders checklist, AS 6669 Plywood sourcing service,phenolic surface film Testing

Grain Raising or Surface SwellingGrain raising is caused by moisture penetrating the phenolic surface film and causingswelling of the surface veneer.The causes of grain raising are: Severe weather exposureFailure to use release agent or form oilDamage to the phenolic surface film i.e. misuse of vibrators, handling damageetc.Faulty phenolic surface filmAs mentioned previously, the purpose of the phenolic surface film is …

Read More »

Staining in Formply,F17 FORMPLY TECHNICAL ,formwork plywood inspection,graders checklist, AS 6669 Plywood sourcing service,phenolic surface film Testing

Staining in FormplyThe most common stains associated with formply are: Rust stainingTannin stainingPinking – free phenol from the phenolic surface film.In the writer’s experience, most staining is due to rust deposits on the deck at the time ofpouring or iron in the aggregate. These stains appear red/brown and are often mistakenfor tannin staining.Tannin staining is the result of extractives from …

Read More »

How to minimise Distortion (Bow and Twist) in Formply,F17 FORMPLY TECHNICAL ,formwork plywood inspection,graders checklist, AS 6669 Plywood sourcing service,

Do not use any new panels showing bow or twist out of the pack. Wheredistortion exceeds 30mm, these panels fail the product standard. They shouldnot be used and returned to the manufacturer.Prevent/Minimise Exposure to MoistureWhere formply panels that have been supplied flat on site distort, there is onlyone cause, this is exposure to moisture, or a change in moisture content.6No …