Quality control in the production process of melamine impregnated paper faced MDF (particleboard),quality assurance,inspection checklist ,factory auditing,sourcing service,Laboratory testing ,inspectors

Quality control in the production process of melamine impregnated paper faced MDF (particleboard) Production process The production process of melamine impregnated paper faced MDF (particleboard) is as follows: substrate preparation → dust removal on the board surface → preforming → hot pressing → trimming → inspection → warehousing.During the production of substrate quality control, the quality of MDF substrate and …

Read More »

Quality defects of melamine impregnated paper faced MDF (patterned board) ,quality assurance,inspection checklist ,factory auditing,sourcing service,Laboratory testing ,inspectors

Common quality defects of melamine impregnated paper faced MDF (patterned board) and their causes 1. Poor physical properties ① Low hot pressing temperature or short hot pressing time, incomplete tree curing, and easy adhesion of dust on the board surface during use, not easy to clean, resulting in dirty surface. ② The hot pressing temperature is too high, the surface …

Read More »

Analysis of factors influencing the quality of melamine impregnated paper panels boards,quality assurance,inspection checklist ,factory auditing,sourcing service,Laboratory testing ,inspectors

Analysis of factors influencing the quality of melamine impregnated paper panels boards Guide: To produce high-quality products, we must select excellent impregnated paper and substrate, and adopt reasonable processing technology; In addition, operators and inspectors should cooperate with each other to control the quality of products, find out the causes of problems and solve them in time, so as to …

Read More »

Cracking of Melamine Paper in Melamine paper Panel ,quality assurance,inspection checklist ,factory auditing,sourcing service,Laboratory testing ,inspectors

Reasons for Cracking of Melamine Paper in Melamine paper Panel Melamine paper will crack in daily use, which is mainly caused by uneven dryness of various parts of wood. In the industry, according to the parts where cracks occur, they are generally called cracks, surface cracks, internal cracks and wheel cracks; The size and number of cracks will vary depending …

Read More »

melamine wood based panels board ,quality assurance,inspection checklist ,factory auditing,sourcing service,Laboratory testing ,inspectors

Methods to judge the quality of melamine wood based panels board (Substrate such as Plywood,Blockboard,MDF ,Particle Board) We can often see the use of melamine wood based panels board (Substrate such as Plywood,Blockboard,MDF ,Particle Board) manufacturers’ products in our daily life. When purchasing wood based panels board (Substrate such as Plywood,Blockboard,MDF ,Particle Board)s, we should check the quality to ensure …

Read More »

Quality defects of melamine facing wood based panels(Substrate such as Plywood,Blockboard,MDF ,Particle Board) ,quality assurance,inspection checklist ,factory auditing,sourcing service,testing

 Poor physical performance The hot pressing temperature is low or the hot pressing time is short, the resin curing is incomplete, and the surface of the melamine paper is easy to stick dust during use, which is difficult to clean and forms a dirty surface. The hot pressing temperature is too high, the hot pressing plates surface temperature is uneven or the …

Read More »

Causes and Prevention Measures of Plywood Bubbling in China,quality inspection checklist,quality control,quality assurance,sourcing specialist ,manufacturing consultant ,factory auditing

Causes and Prevention Measures of Plywood Bubbling in China In the plywood production process, hot pressing is a very important process, which is an important process to finalize the product. It is irreversible. Once quality problems occur, especially bubble will bring great losses to the company. Therefore, it is necessary to understand and master the causes and prevention methods of …

Read More »

Defects easily occurred during hot pressing of plywood in China and solutions,quality inspection checklist,quality control,quality assurance,sourcing specialist ,manufacturing consultant ,factory auditing

Defects easily occurred during hot pressing of plywood in China and solutions 1、 Bubbling and partial delamination Causes: 1. The moisture content of veneer is too high or the drying is uneven 2. Too much glue 3. The pressure drop speed is too fast or the hot pressing temperature is too high 4. Insufficient resin condensation 5. Insufficient hot pressing …

Read More »

Bubbling, delamination , warping, common problems of plywood hot pressing in China,quality inspection checklist,quality control,quality assurance,sourcing specialist ,manufacturing consultant ,factory auditing

Bubbling, delamination , warping, common problems of plywood hot pressing in China 1、 Bubbling and partial delamination Causes: 1. The moisture content of veneer is too high or the drying is uneven 2. Too much glue 3. The pressure drop speed is too fast or the hot pressing temperature is too high 4. Insufficient resin condensation 5. Insufficient hot pressing …