Causes and Prevention Measures of Plywood Bubbling in China,quality inspection checklist,quality control,quality assurance,sourcing specialist ,manufacturing consultant ,factory auditing

Causes and Prevention Measures of Plywood Bubbling in China In the plywood production process, hot pressing is a very important process, which is an important process to finalize the product. It is irreversible. Once quality problems occur, especially bubble will bring great losses to the company. Therefore, it is necessary to understand and master the causes and prevention methods of …

Read More »

Defects easily occurred during hot pressing of plywood in China and solutions,quality inspection checklist,quality control,quality assurance,sourcing specialist ,manufacturing consultant ,factory auditing

Defects easily occurred during hot pressing of plywood in China and solutions 1、 Bubbling and partial delamination Causes: 1. The moisture content of veneer is too high or the drying is uneven 2. Too much glue 3. The pressure drop speed is too fast or the hot pressing temperature is too high 4. Insufficient resin condensation 5. Insufficient hot pressing …

Read More »

Bubbling, delamination , warping, common problems of plywood hot pressing in China,quality inspection checklist,quality control,quality assurance,sourcing specialist ,manufacturing consultant ,factory auditing

Bubbling, delamination , warping, common problems of plywood hot pressing in China 1、 Bubbling and partial delamination Causes: 1. The moisture content of veneer is too high or the drying is uneven 2. Too much glue 3. The pressure drop speed is too fast or the hot pressing temperature is too high 4. Insufficient resin condensation 5. Insufficient hot pressing …