Recent Posts

Staining in Formply,F17 FORMPLY TECHNICAL ,formwork plywood inspection,graders checklist, AS 6669 Plywood sourcing service,phenolic surface film Testing

Staining in FormplyThe most common stains associated with formply are: Rust stainingTannin stainingPinking – free phenol from the phenolic surface film.In the writer’s experience, most staining is due to rust deposits on the deck at the time ofpouring or iron in the aggregate. These stains appear red/brown and are often mistakenfor tannin staining.Tannin staining is the result of extractives from …

Read More »

How to minimise Distortion (Bow and Twist) in Formply,F17 FORMPLY TECHNICAL ,formwork plywood inspection,graders checklist, AS 6669 Plywood sourcing service,

Do not use any new panels showing bow or twist out of the pack. Wheredistortion exceeds 30mm, these panels fail the product standard. They shouldnot be used and returned to the manufacturer.Prevent/Minimise Exposure to MoistureWhere formply panels that have been supplied flat on site distort, there is onlyone cause, this is exposure to moisture, or a change in moisture content.6No …

Read More »

Wrap and Twist in Formply,F17 FORMPLY TECHNICAL ,formwork plywood inspection,graders checklist, AS 6669 Plywood sourcing service,

Wrap and Twist in FormplyAS 6669 provides a 30mm flatness limitation for formply sheets. To measure flatness,formply sheets are placed concave down on a flat surface and any bow or twist exceeding30mm above the flat fails the product Standard.In addition, sheets must be able to be pushed flat using “palm pressure”, of approximately15kg.Formwork plywood supplied to the market with flatness …

Read More »